Just had my 2007 crownline 250cr w/dps-a drive hauled and blocked. when cleaning off the drive I found paint blisters and pealing on top of and under the cavitation plate. boat is equiped with a VOLVO active corrosion module and a Marinepro galvanic isolator. Zinc still have 90% remaining. Should i just sand prime and paint or go back to volvo to plead my case.
tjm
Just had my 2007 crownline 250cr w/dps-a drive hauled and blocked. when cleaning off the drive I found paint blisters and pealing on top of and under the cavitation plate. boat is equiped with a VOLVO active corrosion module and a Marinepro galvanic isolator. Zinc still have 90% remaining. Should i just sand prime and paint or go back to volvo to plead my case.